Raw materials
, General steels, copper and copper alloys, nickel and its alloys
Composition
ag 56 | cu 22 | zn 17 | sn 5 |
Temp. Fusion °C
c.a. 620 – 655°C
Working Temp. °C
c.a. 650 °C
Density
c.a. 9,5 gr/cm3
Tensile strength
430 Mpa
Elongation
25 %
Conducibility
approx. 7,0 m/O mm2 m/O mm2
Technical data
Download PDF
STATE OF SUPPLY
Available
on request

Bar
Ø 0,7 – 9 mm
standard length: 500 mm

coated bars
Ø 1,5 – 2 -3 mm
standard length: 500 mm

Animated wires and bars
ø: 2 – 5 mm
Bars: Length: 500 mm.
threads: skeins or coils

big wires
Ø 0,5 – 5 mm
(in skeins or coils)

fine wires
ø: da 0,3 a 1,4 mm
ø: < 0,4 a request
(in skeins or coils)

rolled strip
thickness 0,1 – 0,9 mm
Width: 2 – 50 mm

rings and preformed
on request

Paste
Ternalloy 56 is an alloy with excellent fluidity and penetration characteristics. It can be used for brazing all steels, copper and copper alloys. Nickel and nickel content alloys. Alloy with low working temperature is recommended for the replacement of Cd content alloys. Mainly used in the production of handcrafted products and in the production of silver products (glasses, silverware, jewelry); in the production of taps; in the field of electronic applications.