Raw materials
General steels, copper and copper alloys, nickel and its alloys
Composition
Ag 30 | Cu 36 | Zn 31,9 | Si 0,1 | Ni 2
Temp. Fusion °C
c.a. 675-790° C
Tensile strength
488 Mpa
Density
c.a. 9,17 gr / cm3
Elongation
36 %
Technical data
Download PDF
STATE OF SUPPLY
Available
on request
Bar
Ø 0,7 – 9 mm
standard length: 500 mm
coated bars
Ø 1,5 – 2 -3 mm
standard length: 500 mm
Animated wires and bars
ø: 2 – 5 mm
Bars: Length: 500 mm.
threads: skeins or coils
big wires
Ø 0,5 – 5 mm
(in skeins or coils)
fine wires
ø: da 0,3 a 1,4 mm
ø: < 0,4 a request
(in skeins or coils)
rolled strip
thickness 0,1 – 0,9 mm
Width: 2 – 50 mm
rings and preformed
Paste
This alloy offers better wettability and possesses excellent mechanical properties at an optimized cost. Suitable for ferrous and non-ferrous base materials. Can be used for brazing carbide tools. The temperature resistance of the weld joints depends on the geometry of the gap and the base metals to be welded. In refrigeration it is recommended for brazing pipes galvanized iron with brass or copper, for the presence of Ni in its composition.